- 9 h before overcoating
- 2К
TRIOCOAT™ ABRASIVE 4600. Modified Epoxy Material
- Provides reliable protection in contact with aggressive substances and under mechanical stress. Has high abrasion resistance and protection against spills of oil, petroleum products, acids, alkalis, and salts.
- Functions effectively in immersion conditions, alternating wetting, as well as in aggressive industrial and marine atmospheres.
- The coating is not demanding on drying times and conditions; it can continue curing even underwater.
- Can be used as an anti-slip floor coating.
TRIOCOAT ABRASIVE 4600 — Technical Data Sheet
Modified epoxy material. Two-component epoxy material with polyamine curing, containing lamellar pigments.
MATERIAL DESCRIPTION
Two-component epoxy material with polyamine curing, containing lamellar pigments.
COATING PURPOSE
Abrasion-resistant coating resistant to spills of oil and petroleum products, non-concentrated solutions of acids, alkalis, salts, intended for anti-corrosion protection in the factory manufacture of metal structures, products and various equipment operated in industrial and marine atmospheres, alternating wetting and immersion zones, petrochemical facilities, ports, offshore and marine projects. The coating is capable of post-curing under water, so immersion in water is allowed soon after application. It is used:
- as a standalone coating;
- with overcoating with polyurethane paint and coating materials in complex anti-corrosion protection systems;
- as part of a special non-slip coating, as a floor coating, on routes for the movement of people and cargo.
The operating temperature in the coating system is from minus 60 to 120 °C.
PHYSICAL CHARACTERISTICS
Recommended thickness of one coat:
| Film thickness | WFT, µm | DFT, µm |
|---|---|---|
| Minimum | 120 | 100 |
| Maximum | 350 | 300 |
It is recommended to obtain the operational coating thickness in 2 or 3 coats.
When used as a non-slip floor coating:
The composition of the coating system is as follows:
| Material name | WFT, µm | DFT, µm |
|---|---|---|
| TRIOCOAT ABRASIVE 4600 | 590 | 500 |
| Abrasive filler * | — | — |
| TRIOCOAT ABRASIVE 4600 | 590 | 500 |
| Acrylic polyurethane materials TRIOTOP FINISH | 110 | 50 |
Note: * — Abrasive filler micromarble Fenix (0.5–2.0) mm (TU 08.12.12-001-45665168-2019) or another in agreement with O3-Coatings LLC must be evenly distributed over the surface of the first coat of TRIOCOAT ABRASIVE 4600. The application technology is according to TI No. 2413/68.
Drying time and overcoating interval:
| Drying time at DFT 200 µm | ||||
|---|---|---|---|---|
| Surface temperature | 5 °C | 20 °C | 30 °C | 40 °C |
| Drying to degree 3 (GOST 19007) | 24 h | 8 h | 6 h | 4 h |
| Drying to degree 6 (GOST 19007) | 72 h | 24 h | 16 h | 10 h |
| Drying to application of the next coat — minimum | 26 h | 9 h | 7 h | 5 h |
| maximum | 6 months | |||
After curing of the coating to degree 3, immersion of the painted structures in fresh water is allowed; after curing to degree 6 — in fresh and sea water.
SURFACE PREPARATION
The material is applied to a prepared metal surface. A typical preparation process includes the following operations: elimination of surface defects to P2 (for operation under corrosivity from C1 to C4 according to ISO 12944-2) or P3 (for operation under corrosivity C5 according to ISO 12944-2) according to ISO 8501-3; degreasing of the surface (if necessary); surface cleaning to grade Sa 2.5 according to ISO 8501-1; during repair and painting of small areas, the use of manual and mechanized cleaning methods to grade St3 according to ISO 8501-1 is allowed; desalting of the surface (if necessary); dust removal of the surface to degree 2 with a particle size of not more than class 2 according to ISO 8502-3. The prepared surface must be dry, and its temperature must be at least 3 °C above the dew point.
APPLICATION
Material preparation:
The material is two-component; before application, the base and the hardener must be mixed separately. The mixing ratio of the base and hardener to obtain a ready-to-apply mixture is 5 : 1 (by volume) (100 : 13.3 by weight). Pot life: 1 h at 20 °C.
Environmental parameters during application:
| Parameter | Value |
|---|---|
| Air temperature | From plus 5 to plus 30 °C |
| Relative air humidity | 10–85 % |
In closed rooms, provide supply-and-exhaust ventilation in the appropriate volume for the period of application and drying.
RECOMMENDED SYSTEMS
Previous coat: none.
Subsequent coat: none or polyurethane paint and coating materials, for example TRIOTOP FINISH 5700.
Note: For this product, as for all epoxy materials, chalking is characteristic during operation without a finish coat outdoors.
STORAGE
24 months from the date of manufacture. It is recommended to store in a dry dark place in sealed factory packaging at a temperature from 0 to plus 30 °C, avoiding direct exposure to UV rays and other heat sources.
TRANSPORTATION
It is recommended to transport at a temperature from 0 to plus 30 °C, avoiding direct exposure to UV rays and other heat sources. Transportation at negative temperatures down to minus 40 °C for a duration of 14 days is allowed.
PACKAGING
Base — 20 l euro pail; Hardener — 5 l euro pail.
HEALTH AND SAFETY
Refer to the Safety Data Sheet for the material.
TRIOCOAT ABRASIVE 4600 — Application Manual
Modified epoxy material. Product description: see Technical Data Sheet for TRIOCOAT ABRASIVE 4600.
CONTENTS
The instruction provides guidance on surface preparation; material preparation for application; the application process and equipment used; storage conditions; safety precautions; fire safety measures; environmental protection; first aid measures.
SURFACE PREPARATION
The material is applied to a prepared and dry metal surface with a temperature at least 3 °C above the dew point. The required degree of surface preparation depends on the predicted operating conditions and service life, and design requirements.
A typical preparation process includes the following operations: elimination of surface defects to P2 (for operation under corrosivity from C1 to C4 according to ISO 12944-2) or P3 (for operation under corrosivity C5 according to ISO 12944-2) according to ISO 8501-3; degreasing of the surface (if necessary); surface cleaning to grade Sa 2.5 according to ISO 8501-1 with a recommended roughness profile of 50–75 µm; during repair and painting of small areas, the use of manual and mechanized cleaning methods to grade St 3 according to ISO 8501-1 is allowed; desalting of the surface (if necessary); dust removal of the surface to degree 2 with a particle size of not more than class 2 according to ISO 8502-3.
MATERIAL PREPARATION
TRIOCOAT ABRASIVE 4600 is a two-component epoxy material with polyamine curing, containing lamellar pigments, with volume solids (85±5) %.
The material is supplied in euro pails: base — 20 l euro pail, hardener — 5 l euro pail.
After opening the container, before application, the base and the hardener must be mixed separately. Mixing is carried out in a ratio of 5 : 1 (base : hardener) by volume (100.0 : 13.3 by weight).
APPLICATION
Application method:
Airless spraying / Manual application.
Thinner:
Thinner TRIOSOLV 0002 (if necessary), up to 10 % by volume for airless spraying. For more detailed information, contact O3-Coatings.
Nozzle diameter (recommended):
.019"–.025"
Operating pressure (recommended):
Not less than 150 bar.
Equipment cleaning:
Thinner TRIOSOLV 0002 (other solvents may be used in agreement with O3-Coatings).
Table 1 — Recommended application conditions
| Recommended application conditions | Value |
|---|---|
| Air temperature | From plus 5 to plus 30 °C |
| Relative air humidity | (10–85) % |
In closed rooms, it is necessary to provide supply-and-exhaust ventilation in the appropriate volume for the period of application and drying.
Before the start of each work shift, it is recommended to check and record the following parameters:
- environmental conditions (air temperature, relative humidity);
- dew point temperature;
- surface temperature;
- absence of moisture and oil contamination on the surface;
- absence of dust on the surface.
Before applying the material, pass a solvent through the spray equipment to clean it from previously used paints and coatings. The solvent depends directly on the type of materials used earlier. Equipment cleaning is also recommended at the end of the work shift.
The material should be applied by airless spraying; application with a brush or roller is allowed in hard-to-reach places or on small surfaces.
The recommended thickness of one coat is given in Table 2.
Table 2 — Recommended thicknesses of TRIOCOAT ABRASIVE 4600
| Film thickness | WFT, µm | DFT, µm |
|---|---|---|
| Minimum | 120 | 100 |
| Maximum | 350 | 300 |
It is recommended to obtain the operational coating thickness in 2 or 3 coats.
Pot life of the material — 1 h at 20 °C.
When used as a non-slip floor coating, the composition of the coating system is as follows:
| Material name | WFT, µm | DFT, µm |
|---|---|---|
| TRIOCOAT ABRASIVE 4600 | 590 | 500 |
| Abrasive filler * | — | — |
| TRIOCOAT ABRASIVE 4600 | 590 | 500 |
| Acrylic polyurethane coating TRIOTOP FINISH | 110 | 50 |
Note: * — Micromarble Fenix (0.5–2.0) mm (TU 08.12.12-001-45665168-2019) or another in agreement with O3-Coatings LLC may be used.
The consumption of the recommended abrasive filler micromarble Fenix is (1.35±0.10) kg/m². The actual consumption is determined by the project requirements and the type of filler used, but not less than 0.5 kg/m².
The application procedure consists of the following operations:
- Manually distribute the abrasive filler in a uniform layer over the surface of the first coat of TRIOCOAT ABRASIVE 4600, immediately after applying the paint and coating material, completing the process within 0.5 h. Do not roll the abrasive filler;
- If it is necessary to move over the coating, it is recommended to walk using specialized shoes for working on self-leveling floors, equipped with spikes (paint boots).
Formation of the layer of TRIOCOAT ABRASIVE 4600 with abrasive filler at plus (20±2) °C is 24 h. After this time, before applying the second coat of TRIOCOAT ABRASIVE 4600, the remains of the abrasive filler not fixed in the first coat of the coating material are removed from the surface using an industrial vacuum cleaner.
The drying time of the material TRIOCOAT ABRASIVE 4600 is given in Table 3.
Table 3 — Drying time of TRIOCOAT ABRASIVE 4600 at DFT 200 µm
| Surface temperature | 5 °C | 20 °C | 30 °C | 40 °C |
|---|---|---|---|---|
| Drying to degree 3 (GOST 19007) | 24 h | 8 h | 6 h | 4 h |
| Drying to degree 6 (GOST 19007) | 72 h | 24 h | 16 h | 10 h |
| Drying to application of the next coat — minimum | 26 h | 9 h | 7 h | 5 h |
| maximum | 6 months | |||
After curing of the coating to degree 3, immersion of the painted structures in fresh water is allowed; after curing to degree 6 — in fresh and sea water.
The drying times given in this section are for guidance only. When assessing the actual drying time, it is also necessary to take into account the presence of air flows and relative air humidity.
Wet film thickness is controlled with a "comb" gauge using the last tooth touching the paint. Above each tooth of the comb, its gap value in microns from the "base" teeth (from 0) is marked.
When performing measurements, the comb must be installed perpendicular to the plane of the painted surface. After each measurement, the surface of the comb in contact with the paint must be thoroughly wiped with a clean cloth.
The wet film thicknesses of the coating must be recorded.
Quality control of the finished coating is performed according to the following characteristics:
- appearance (no sags, cracking, peeling, etc.) — a uniform grey coating;
- dry film thickness is determined by the 80–20 rule: 80 % of the measured thicknesses must be not less than the thickness specified in the specification (nominal thickness); 20 % of the measured thicknesses must be not less than 80 % of the nominal thickness.
STORAGE
It is recommended to store the material TRIOCOAT ABRASIVE 4600 in a dry dark place in sealed factory packaging at a temperature from plus 0 to plus 30 °C, avoiding direct exposure to UV rays and other heat sources.
The shelf life of TRIOCOAT ABRASIVE 4600 is 24 months from the date of manufacture.
TRANSPORTATION
It is recommended to transport at a temperature from 0 to plus 30 °C, avoiding direct exposure to UV rays and other heat sources. Transportation at negative temperatures down to minus 40 °C for a duration of 14 days is allowed.
SAFETY PRECAUTIONS
General provisions:
During work, the requirements of GOST 12.3.002, GOST 12.3.005, GOST R 12.3.052 must be observed.
Hazardous and harmful production factors must be eliminated or reduced to acceptable levels.
When organizing and performing painting work, physiologically justified work and rest regimes should be provided.
Personnel requirements:
Persons not younger than 18 years of age who have completed the following are allowed to perform anti-corrosion works:
- occupational safety training — according to Decree of the Government of the Russian Federation No. 2464 of 24 December 2021, industrial sanitation, fire and electrical safety;
- vocational training.
Officials, in accordance with the requirements of SNiP 12-03 and SNiP 12-04, are responsible for compliance with labour protection and industrial safety requirements during work.
Workers must know:
- hazardous and harmful production factors, harmful substances in the composition of the materials used in the air of the working zone and the nature of their effect on the human body;
- instructions on the procedure for performing work and maintaining the workplace;
- instructions on labour protection, fire safety, industrial sanitation;
- personal hygiene rules;
- rules for the use of personal protective equipment (PPE);
- rules for providing first aid.
Safety requirements for surface preparation and painting:
All work related to the use of paints and coatings in rooms must be carried out with operating general supply-and-exhaust and local exhaust ventilation according to GOST 12.4.021. Ventilation must ensure that the content of harmful substances in the air of the working zone does not exceed the maximum permissible concentrations in accordance with the requirements of GOST 12.1.005, SanPiN 1.2.3685.
Workers engaged in surface degreasing, preparation and application of paints and coatings must be provided with the following PPE:
- protective painting suits, disposable or reusable, with a zipper running along the length of the garment for ease of putting on and taking off, elastic bands at the wrists, ankles and waist, and a hood;
- technical rubber gloves according to GOST 20010;
- safety glasses according to GOST 12.4.253 (EN 166:2002), symbol 3, or equivalent with the same functional purpose;
- filtering respirators with an insulating face piece in the form of a half-mask according to GOST 12.4.296 with a combined RPE filter providing simultaneous protection against gases, vapours and aerosols according to GOST 12.4.235 AZRZ (brown-white), AKhRZ or equivalent with the same functional purpose;
- footwear made of leather, with a hard toe to avoid injury to the feet in case of falling heavy objects; the sole is protected by a metal plate.
Storage of organic solvents at the workplace is allowed in hermetically sealed containers in an amount not exceeding the two-shift norm.
When working with solvents, observe the following safety requirements:
- use respiratory and eye PPE;
- work with the ventilation system turned on, providing air exchange at the required rate.
During surface preparation, the sandblaster must work in special clothing made of dust-proof fabric and a helmet of the MIOT-49 type, and use PRB-5 respirators with forced air supply.
Rules for handling toxic substances:
The material TRIOCOAT ABRASIVE 4600 is manufactured in accordance with TU 20.30.12-295-40141638-2025.
The container in which the material TRIOCOAT ABRASIVE 4600 is located must have a label with the exact name and designation of the material contained in it. The container must be intact and have a tightly closing lid.
In case of accidental spillage of material, cover the spill area with sawdust or sand, having previously protected the respiratory organs. Contaminated solvents, sawdust, sand, rags, cloths should be collected in buckets and removed to specially designated places in accordance with the requirements of GOST 30772, GOST R 52107.
Eating and smoking is allowed only in specially designated places.
FIRE SAFETY MEASURES
Fire safety measures during painting work must be carried out in accordance with the Technical Regulation on Fire Safety Requirements (No. 123-FZ of 22 July 2008) and other regulatory documents.
The paints and coatings used are classified as flammable materials; therefore, fire safety measures are taken at the workplace in accordance with the requirements of GOST 12.1.004 and Decree of the Government of the Russian Federation No. 1479 of 16.09.2020 "On Approval of the Fire Regime Rules in the Russian Federation".
When performing surface preparation for painting and painting works, it is not allowed to:
- smoke, light fires, or carry out welding works within a radius of 25 m from the work site, as well as along the entire vertical in this zone;
- heat production rooms and protected objects with electrical appliances of standard design.
In the event of a fire, people should be evacuated from the danger zone, the fire service should be notified, paints and coatings should be removed from the work zone, and fire extinguishing should be started with the available means in strict accordance with the approved plan.
ENVIRONMENTAL PROTECTION
During painting work, solid and liquid wastes are generated, as shown in Table 4.
Table 4
| Waste name | Waste disposal method |
|---|---|
| Solid waste: material container — euro pails | Dispose of containers as household waste. Euro pails can be used for technical purposes after the material has dried on the inner walls. |
| Liquid waste: solvent/cleaner for flushing painting equipment; material residues | Disposed of by the work manufacturer in accordance with GOST 30772, GOST R 52107. |
FIRST AID MEASURES
General:
If poisoning is suspected, seek medical help.
In case of inhalation:
If the product is inhaled, move the victim to fresh air, ensure rest and seek medical help.
In case of contact with eyes:
If the product gets into the eyes, rinse them with plenty of clean running water and seek medical help.
In case of contact with skin:
If the product gets on the skin, remove contaminated clothing and wash the contact area thoroughly with soap and water. The use of solvents or thinners is prohibited.
In case of contact with food:
If the product enters the body with food, ensure rest for the victim and immediately seek medical help.
You may also be interested in
TRIOTOP™ FINISH 5720
Two-component acrylic polyurethane enamel
Application temperature : -10°С/+35°С
Color : RAL color matching
TRIOTOP™ FINISH 5300
Single-pack fast-drying enamel based on a synthetic film-forming agent
Application temperature : -30°С / +30°С
Color : RAL color matching
TRIOCOAT™ PRIMER 1300
One-component fast-drying primer based on a synthetic film-forming agent
Application temperature : -30°С / +30°С
Color : RAL color matching , Gray , Red‑brown
Any questions?